Fortiflex® HDPE K46-06-161 HDPE Copolymer with Carbon Black
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: Innovene is a wholly owned subsidiary of BP Group. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Key Words: High Density Polyethylene
Material Notes: Fortiflex® K46-06-161 is a precompounded black (0.20% Carbon Black), high molecular weight, high density copolymer polyethylene developed for automotive fuel tanks. When surface treated, this material exhibits excellent resistance to permeation of gasoline and gasoline/alcohol blends. It also combines excellent processability and outstanding physical performance, particularly environmental stress crack resistance (ESCR) and impact properties.This product information was provided by Solvay Polymers, now a part of the BP Solvay Polyethylene North America joint venture (Nov. 2001).
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|