Fortiflex® HDPE 50-1000 HDPE Copolymer, Narrow MW Distribution
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: This product is not listed in the standard Innovene product line. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Key Words: High Density Polyethylene
Material Notes: Fortiflex® T50-1000 is a high density polyethylene copolymer. It has a narrow molecular weight distribution and provides injection molded parts with an excellent balance of properties and processing for most general purpose applications. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. This resin is Kosher certified.This product information was provided by Solvay Polymers, now a part of the BP Solvay Polyethylene North America joint venture (Nov. 2001).
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|