Fortiflex® HDPE B53-35H-FLK, Blow Molding Grade Polyethylene

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Close Analogs: Innovene is a wholly owned subsidiary of BP Group. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.

Material Notes:
A high density polyethylene copolymer flake developed for blow molding applications which contains no additives and is not pelletized. It is recommended for use in applications which require a combination of high top load strength and good ESCR. This material meets the FDA requirements of 21CFR 177.1520. This resin is Kosher certified.

This product information was provided by Solvay Polymers, now a part of the BP Solvay Polyethylene North America joint venture (Nov. 2001).

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Izod Impact, Notched
  • Tensile Impact Strength
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。