Ineos HDPE K38-20-188
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Material Notes: A natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural gas distribution. The resulting formulation, known as K38-20-160, is recognized by the Plastics Pipe Institute as having a PE2406 and PE80 rating. It exhibits excellent long term stress life and outstanding environmental stress crack resistance. Cell Classification 234360D.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- PENT
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|