Ineos HDPE T50-800
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Close Analogs: Innovene is a wholly owned subsidiary of BP Group. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Key Words: Good balance of processability and end-use properties
Material Notes: A high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use properties are required. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. This resin is Kosher certified.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|