Ineos HDPE TC46-20
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Close Analogs: Innovene is a wholly owned subsidiary of BP Group. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Key Words: Toughness, crush strength, and processability
Material Notes: A natural high density polyethylene copolymer designed specifically for telecommunications ducting. TC46-20 balances stiffness, ESCR, and molecular weight to provide required toughness and crush strength without compressing processability.Cell classification is 335440A per ASTM D 3350. Oxidative Induction Time is 20 min at 200°C per ASTM D3895.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Oxidative Induction Time (OIT)
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|