Ineos HDPE K44-15-122
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Close Analogs: Innovene is a wholly owned subsidiary of BP Group. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Key Words: Meets ANSI/NSF Standard
Material Notes: A natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF Standard 61 health effects requirements, and is recognized by the Plastic Pipe Institute as having a pipe material designation code of PE 3408. A pressure rated formulation is also produced when this product is extruded in combination with a Ineos Polyethylene approved black masterbatch. The resulting formulation known as K44-15-123 has NSF Standard 14 certification and complies with ANSI/NSF Standard 61 health effects requirements, is certified to CSA Standard B137.1-99 and B137.4-99, and is listed with the Plastic Pipe Institute as a PE3408. The hydrostatic design basis is 1600 psi at 23°C, based on ASTM test number D 2837. According to ASTM F 1473, the notch tensile (PENT) is greater than 100 hours. Also, the cell classification is 345464A (ASTM D3350).
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- PENT
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Hydrostatic Design Basis @ 73°F
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|