BP Amoco Fortilene® TG 6801 Polypropylene Copolymer, High Impact
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: This product is not listed in the standard Innovene product line. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortilene® Polypropylene product line from Solvay Polymers in November 2001.
Key Words: PP
Material Notes: Fortilene® TG 6801 belongs to the new generation of Solvay polypropylenes produced by gas phase polymerization. This high impact copolymer is intended for injection molding of automotive parts, furniture, etc. This material meets the FDA requirements of 21CFR 177.1520. Data provided by the manufacturer, Solvay Polymers, Inc.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Low Temperature Gardner Impact
- Dart Drop Test
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|