BP Amoco Fortilene® PP KB4187, Blow Molding/Extrusion Grade Polypropylene
Subcategory: Polypropylene; Thermoplastic
Close Analogs: This product is not listed in the standard Innovene product line. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortilene® Polypropylene product line from Solvay Polymers in November 2001.
Material Notes: An antistated, clarified polypropylene random copolymer produced by Solvay Polymers utilizing catalyst technology. It is designed for blow molding and extrusion applications where high impact resistance and excellent clarity are performance requirements. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. This resin is Kosher certified. Information provided by Solvay Polymers.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|