Innovene L57N-00 Injection Grade Polypropylene
Subcategory: Polypropylene; Thermoplastic
Close Analogs: The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortilene® Polypropylene product line from Solvay Polymers in November 2001.
Material Notes: Formerly BP Amoco Fortilene® PP RG7910. Belongs to the new generation of Solvay polypropylenes produced by gas phase polymerization. This medium impact nucleated copolymer is intended for injection molding of household goods, packaging articles, etc. This resin is Kosher certified. This material meets the FDA requirements of 21CFR 177.1520 and U.L. 94HB flammability rating. Information provided by Solvay Polymers.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Low Temperature Gardner Impact
- Impact Test
- Melting Point
- Crystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|