BP Amoco Fortilene® PP SG6812 Polypropylene

 

Subcategory: Polypropylene; Thermoplastic

Close Analogs: This product is not listed in the standard Innovene product line. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortilene® Polypropylene product line from Solvay Polymers in November 2001.

Material Notes:
Belongs to the new generation of Solvay polypropylenes produced by gas-phase polymerization. This reactor-made thermoplastic olefin is intended for automotive applications that require excellent processability and very high impact resistance at low temperatures. Meets FDA requirements of 21 CFR 177.1520 and is approved by U.L. for their 94HB-flammability rating.

Information provided by Solvay Polymers.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Yield
  • Flexural Modulus
  • Izod Impact, Notched
  • Izod Impact, Notched, Low Temp
  • Low Temperature Gardner Impact
  • Impact Test
  • Melting Point
  • Crystallization Temperature
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。