Solvay Advanced Polymers Torlon® 5030 Polyamide-Imide, 30% Glass Fiber Filled
Subcategory: Polyamide-imide; Thermoplastic; Polymer
Key Words: PAI
Material Notes: High stiffness, good retention of stiffness at elevated temperature, very low creep, and high strength. Used for: Burn-in sockets, gears, valve plates, fairings, tube clamps, impellers, rotors, housings, back-up rings, terminal strips, insulators, and brackets. Information provided by Solvay Advanced Polymers.
| Available Properties |
- Density
- Water Absorption
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Compressive Modulus
- Poissons Ratio
- Shear Modulus
- Shear Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|