Solvay Advanced Polymers Acudel™ 22000 Polyphenylsulfone Blend
Subcategory: Polyphenylsulfone; Thermoplastic
Close Analogs: Information provided by Solvay Advanced Polymers.
Material Notes: ACUDEL 22000 is a polyphenylsulfone-based polymer blend. It is a high-heat, high-performance resin formulation exhibiting very good hydrolytic stability, excellent resistance to acids and bases, and good resistance to stress cracking under a broad range of chemical environments. In addition to these attributes, ACUDEL 22000 resin exhibits robust toughness and improved notch resistance compared to both UDEL® polysulfone and RADEL® A polyethersulfone, although slightly lower than that of neat RADEL® R polyphenylsulfone. In general, the performance profile of ACUDEL 22000 resin is intermediate between that of polysulfone and polyphenylsulfone. In addition to its high mechanical and thermal performance attributes, ACUDEL 22000 resin also offers very good electrical properties over a broad temperature range as well as inherent flame retardancy. The material exhibits excellent flow characteristics and can be readily processed using conventional injection molding equipment. The “natural” version of ACUDEL 22000 is designated ACUDEL 22000 NT15 and its color is an opaque light beige. It is available in black as ACUDEL 22000 BK937 resin. ACUDEL 22000 resin can also be made available in a variety of colors.
| Available Properties |
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Tensile Impact Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|