Solvay Advanced Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer
Subcategory: Liquid Crystal Polymer (LCP); Thermoplastic
Close Analogs: Information provided by Solvay Advanced Polymers.
Material Notes: XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder temperatures. The heat deflection temperature of this resin is 568°F (298°C) and the moldability is exceptional. XYDAR G-430 resin can fill very thin walls over long flow lengths with little or no flash, even at mold temperatures below 200°F (93°C). In addition, it has low warpage in molded products and exceptional weld line strength. Like other XYDAR Liquid Crystal Polymers, this material exhibits high strength and stiffness (even at elevated temperatures), low coefficient of thermal expansion, high deflection temperature, inherent flame resistance, and outstanding resistance to most chemicals, weathering, and radiation. This resin is particularly well suited for many applications that have difficult-to-fill geometries, and require resistance to warp, strong weld lines, and compatibility with IR reflow environments. Potential applications for this resin include electronic connectors, surface mount interconnection devices, sockets, and PCMCIA card frames.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Dew Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|