Solvay Advanced Polymers Xydar® MG-350 Liquid Crystal Polymer, Mineral and Glass Filled
Subcategory: Liquid Crystal Polymer (LCP); Thermoplastic
Close Analogs: Information provided by Solvay Advanced Polymers. This grade was discontinued in 2006.
Material Notes: XYDAR MG-350 Liquid Crystal Polymer (LCP) is a mineral and glass-filled injection molding grade developed specifically for cost-effective performance in applications where a balance of flatness and strength are required. The moldability of this resin is exceptional. XYDAR MG-350 resin can fill very thin walls over long flow lengths with little or no flash, even at mold temperatures below 200°F (93°C). In addition, it has low warpage in molded products and good weld line strength. Like other XYDAR Liquid Crystal Polymers, this material temperatures), low coefficient of thermal expansion, high deflection temperature, inherent flame resistance, and outstanding resistance to most chemicals, weathering, and radiation. This resin is particularly well suited for many applications that have difficult-to-fill geometries, and require resistance to warp and strong weld lines. Potential applications for this resin include electronic connectors, burn-in sockets, automotive components, chemical processing and other mechanical devices.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact Unnotched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Dew Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|