SolVin® 172GA Polyvinyl Chloride Emulsion Polymer
Subcategory: Vinyl; Thermoplastic
Key Words: PVC
Material Notes: Made by emulsion polymerization.
APPLICATIONS
Calendering : plasticized films and sheets
Extrusion : rigid or plasticized pipes and profiles
In most cases, SolVin 172GA resin is used in blends with suspension resins Information provided by SolVin.