SolVin® 173GB Polyvinyl Chloride Emulsion Polymer

 

Subcategory: Vinyl; Thermoplastic

Key Words: PVC

Material Notes:
Made by emulsion polymerization.

APPLICATIONS
Calendering :
plasticized films and sheets
Extrusion : rigid or plasticized pipes and profiles
In most cases, SolVin 173GB resin is used in blends with suspension resins.
CHARACTERISTICS
SolVin 173GB is a polyvinyl chloride with a high K value, supplied in the form of a white powder consisting of cenospheres.
SolVin 173GB includes polymerization additives which make it easier to process. Its intrinsic thermal stability is high.
Compared with suspension polymers having the same viscosity index, SolVin 173GB resin permits lower processing temperatures and more rapid gelation ("processing aid" effect).
SolVin 173GB resin imparts "handle" to plasticized calendered films and gives good impact strength to rigid extruded products.

Information provided by SolVin.

Available Properties
  • Volatile Organic Compounds (VOC) Content
  • Apparent Bulk Density
  • Particle Size
  • Viscosity Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。