Solvay Solexis Solef® 31008 PVDF Copolymer
Subcategory: Fluoropolymer; Thermoplastic; PVDF
Key Words: Polyvinylidene Fluoride
Material Notes:
Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules. General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystalline thermoplastic which is obtained by polymerizing vinylidene fluoride. Important properties include excellent chemical resistance to most aggressive substances and solvents, excellent mechanical strength and toughness, high abrasion resistance, high temperature capabilities, excellent aging resistance, high purity, resistance to UV and nuclear radiation, excellent intrinsic fire resistance, resistance to weathering, low permeability to most gases and liquids, and easily melt-processed by standard methods of molding and extrusion. Tensile properties are achieved with varying methods of sample fabrication. Information provided by Solvay Solexis, Inc.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Coefficient of Friction
- Coefficient of Friction, Static
- Taber Abrasion, mg/1000 Cycles
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Heat of Fusion
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Crystallization Temperature
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Brittleness Temperature
- Glass Temperature
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|