Spartech APET SP4110 Copolyester Sheet
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Description: Copolyester Sheet Information provided by Spartech.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Unnotched
- Falling Dart Impact
- Izod Impact, Unnotched @ -40°C
- CTE, linear 68°F
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Gloss
|
|
|
|
| Property Data |