Spartech LDPE SP-1310 Polyolefin Sheet
Subcategory: Polyethylene; Polyolefin; Thermoplastic; LDPE
Material Notes: Description: Polyolefin Sheet Information provided by Spartech.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Dart Drop
- CTE, linear 68°F
|
|
|
|
| Property Data |