Spartech Noryl® GTX SP-52Z1 Structural Sheet
Subcategory: Polyphenylene Ether/PPO; Thermoplastic
Material Notes: Description: Structural Sheet Noryl is a registered trademark of General Electric Company. Information provided by Spartech.