Spartech Ultros SRP Co-Extruded Skid-Resistant PE Specialty Sheet
Subcategory: Polyethylene; Thermoplastic
Material Notes: Description: Specialty Sheet Information provided by Spartech.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- CTE, linear 68°F
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|