STAR Starflex® Optiflex P 7055-1002 Thermplastic Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Description: Starflex Optiflex P 7055-1002 represents the latest development in "ultra-clear" TPE technology. It has been developed for injection molding applications requiring high-clarity and light transmission. Applications: Super clear, grip, button Information provided by STAR Thermoplastic Alloys & Rubbers.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Shore A
- Rear Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Injection Pressure
- Back Pressure
- Color
- Injection Rate
|
|
|
|
| Property Data |