Saint-Gobain Norton® T-200 Mechanical Grade PTFE Sheet (0.062" thick)
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes: Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate release sheets, wire and cable wrap, and industrial gasketing.
PTFE = polytetrafluoroethylene
T-200 is a mechanical grade PTFE sheet manufactured from reground PTFE. It is available in thicknesses ranging from 0.015" to 0.250" and standard widths of 12", 24", 36", and 48". PTFE film is supplied either in sheet or continuous roll form. Slit widths are available in thicknesses ranging from 0.001" to 0.062" and to the exacting tolerances of the wire and cable, and electronics industries. Custom colors are also available.
Types of application include Electrical/Electronics, Medical, and Protective/Decorative
Specification Notes: T-200 sheet meets the physical requirements of AMS 3651C. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Specific Gravity
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- CTE, linear 68°F
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|