Saint-Gobain Norton® FEP Fluoropolymer Film

 

Subcategory: Fluoropolymer; Thermoplastic; FEP; Polymer

Material Notes:
Features/Benefits:

  • Outstanding clarity
  • Outstanding anti-stick release properties
  • Performance from -254°C (-425°F) to 205°C (400°F)
  • Exceptional chemical resistance and electric properties
  • Complies with FDA requirements
  • Product thicknesses from 0.0005" to 0.010" and up to 48" for over 0.010" thick
  • Optically transparent and pigmented
  • All films are manufactured and converted in class 100,000 clean room facility
  • Available in cementable (surface treated) form

Norton® FEP fluoropolymer film is manufactured from fluorinated ethylene propylene (FEP) resin by Saint-Gobain Advanced Films and Fabrics in four grades.

Norton® FEP Type FG utilizes the low dielectric constant and dissipation over a wide range of temperatures and frequencies for low signal distortion and attenuation in flexible printed circuit and flat cable applications. The high surface and volume resistivity minimizes current leakage and provides excellent insulation in wire and cable applications.

Norton® FEP also provides the chemical and thermal resistance to withstand aggressive environments, making it an excellent candidate for diaphragms, gaskets, protective linings, sample bags, and containers. Fabricated shapes and contours can be produced via heat sealing and thermoforming. The outstanding weatherability and optical properties of Norton® FEP film provide excellent performance in environmental growth chambers and solar collectors.

Norton® Type FS is a translucent film made from high molecular weight resin for applications where high flex life and stress-crack-resistant performance are required, such as tank linings and diaphragms.

Norton® FEP Type RF is a clear or pigmented film designed for release applications. The non-stick surface, chemical resistance, and 205°C (400°F) usage temperature make Norton® FEP an ideal release film for composite molding over a wide range of resin systems. High elongation and a smooth, low-gel film surface allow Norton® FEP to to conform to complex mold contours and produce a smooth part finish. Perforated film is available to control outgassing and resin bleed. Pigmented films increase visibility to speed removal from parts and mold.

Norton® FEP Type WF (mechanical grade) film is an ideal economical solution for applications that don't require high aesthetic standards, such as hot melt adhesive (welding tape) application. FEP WF film possess all physical, mechanical, and thermal properties of FEP FG grade, while offering up to 15% savings.

Surface Treatments Available: C-Treatable (cementable, 1 or 2 sides); Corona Treatment (1 or 2 sides); Chemical Etching (1 or 2 sides)
Flammability (UL-94) = V - 0
Used for Aerospace/Release Films, Chemical Process, Electrical/Electronics, Medical, Protective/Decorative.

Specification Notes: All values represent typical performance properties and should not be used for specification purposes.
Information provided by Saint Gobain Performance Products.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Tear Strength
  • Elmendorf Tear Strength, MD
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 68°F
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  • Refractive Index
  • Transmission, Visible
  • Fold Endurance (MIT) (cycles)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。