Saint-Gobain Norton® ECTFE Fluoropolymer Film

 

Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE; Polymer

Material Notes:
Features/Benefits:

  • Outstanding release properties
  • Performance from -200°C (-328°F) to 165°C (330°F)
  • High dielectric strength
  • Excellent chemical, radiation, weather and abrasion resistance
  • Non-flammable
  • Thermoformable
  • Product thicknesses from 0.0005" (0.013 mm) to 0.010" (0.254 mm)
  • Width up to 60" (1524 mm)
  • Blue, clear, and white colors
  • All films are manufactured and converted in class 100,000 clean room facility

Norton® ECTFE fluoropolymer film is manufactured from ethylene-chlorotrifluoroethylene (Halar®, a registered trademark of Ausimont USA, Inc) resin by Saint-Gobain Advanced Films and Fabrics. This material offers the outstanding performance of fluoropolymer film over a temperature range from cryogenic -200°C (-328°F) to 165°C (330°F).

Norton® ECTFE film provides the highest abrasion resistance of any fluoropolymer film available. This film has superior chemical resistance and very high tensile strength and flexural modulus.

Norton® ECTFE film offers low surface energy, making it an excellent choice for release applications. The low specific gravity of ECTFE provides more square feet than FEP for composite fabrication.

The combination of heat stability, electrical characteristics, and barrier properties provides insulator performance especially suited for the electrical and electronics industry. Norton® ECTFE film offers the highest dielectric strength of all fluoropolymer films.

Norton® ECTFE film has outstanding resistance to weathering and high energy radiation. This material is suited for electrical tapes, cable insulation, printed circuits, capacitors, chlorine cells, flat cable constructions, and solar collectors.

Norton® ECTFE film offers a UL V-0 rating for flammability. This provides performance suitable for aircraft cabin interiors and fuel cell membranes.
Used primarily for Aerospace/Release films, Chemical Process, Electrical/Electronics
Information provided by Saint Gobain Performance Products.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Tear Strength
  • Elmendorf Tear Strength, MD
  • Heat Seal Strength Initiation Temperarture
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 68°F
  • Melting Point
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Refractive Index
  • Fold Endurance (MIN)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。