Saint-Gobain Norton® ETFE Fluoropolymer Film
Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE; Polymer
Material Notes: Features/Benefits:
- Superior release properties
- Excellent weatherability
- Performance from -200°C (-328°F) to 165°C (330°F)
- Excellent chemical and mechanical properties
- Thermoformable
- Product thicknesses from 0.0005" (0.0127 mm) to 0.020 (0.5 mm)
- Width up to 62" (1575 mm) for 0.0005" to 0.010" and up to 48" for 0.010" - 0.020"
- Blue, red and custom colors available
- Available in cementable (surface treated) form
High Yield Fluoropolymer Film Norton® ETFE fluoropolymer film is manufactured from a copolymer of ethylene and tetrafluoroethylene resin. This material offers the outstanding performance of fluoropolymer film over a temperature range from cryogenic to 165°C (330°F). The resistance to chemicals and weathering, low flammability, and stress crack resistance make this film an excellent candidate for a wide variety of applications.
Weatherable Applications Norton® ETFE film offers excellent mechanical properties and tear resistance. The high light transmission (>95%) of Norton® ETFE film, when combined with its excellent mechanical and chemical properties, provides excellent performance in architectural roofing designs and greenhouses. Norton® ETFE film is also an excellent choice in solar collector applications due to its outstanding physical properties and high coverage factor resulting from its low density.
Low Surface-energy Applications Norton® ETFE film offers a low surface energy, making it an excellent choice for release applications up to 350°F process temperature. The low density of this material, compared to Norton® FEP film, provides greater coverage per pound for composite molding release film applications. The low surface energy of Norton® ETFE can also be utilized in applications such as wall coverings and anti-graffiti protection for high traffic areas.
Fabrication Capabilities Norton® ETFE film offers processors excellent dimensional stability for secondary processing such as thermoforming and welding. Products utilizing Saint-Gobain's surface treatment technologies, such as C-treatment, improve bondability characteristics for metalizing processes and adhesive coating.
Surface Treatments Available: C-Treatable (cementable, 1 or 2 sides); Corona Treatment (1 or 2 sides); Chemical Etching (1 or 2 sides) Flammability (UL-94) = V-0 Used for Aerospace/Release Films, Chemical Process, Electrical/Electronics, Medical, Protective/Decorative.
Specification Notes: All values represent typical performance properties and should not be used for specification purposes. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Specific Gravity
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Elmendorf Tear Strength, MD
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
- Refractive Index
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|