Saint-Gobain Rulon® 957 Grade Bearing/Seal PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE; Polymer;
Material Notes: Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are used in bearing and seal applications from temperature extremes of 400°F to over 500°F with and without additional lubricants. A unique property of Rulon® is the absence of stick slip, that is, erratic low-speed motion. PTFE = polytetrafluoroethylene
957 Grade Bearing/Seal PTFE: Low friction/wear against coated metal or porcelain surfaces. Appropriate mating surfaces are steel, Rc 25 or higher, or painted metal/porcelain. Suitable for use in environments of steam, wet, dry, or vacuum type. Green in color. Material has electrical and thermal insulation properties. Information provided by Saint Gobain Performance Products.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|