Saint-Gobain Norton® Tygon® High Purity Tubing Formulation 2275
Subcategory: Thermoplastic
Material Notes: Description: Tygon® 2275: Tygon® High Purity Tubing is ideal for handling sensitive fluids such as pharmaceutical or biological solutions. There is virtually no absorption of key fluid constituents into the tubing material or fluid adsorption onto the tubing walls. As a result, fluid alteration and loss is limited. There is no plasticizer to leach into or contaminate the fluid, yet the tubing remains flexible. Tygon® High Purity Tubing can be sterilized by radiation, ethylene oxide, steam or chemical methods. Frequently, incineration is used to dispose of contaminated materials. While many tubings release hazardous by-products when burned, Tygon® High Purity Tubing only releases carbon dioxide and water when properly incinerated, providing safe disposal. Also available with reinforcement to withstand elevated working pressure.
Features and Benefits:- Exceptionally low absorption and adsorption compared to silicone
- Smooth inner surface inhibits particulate entrapment
- Environmentally safer to dispose; reduces cost of disposal
- Highly resistant to aggressive cleaners and sanitizers
- Plasticizer free
- Meets USP Class VI and FDA requirements for Food Contact
Typical applications include Sterile Filling and Dispensing Systems, Diagnostic Equipment, Nuclear Equipment, Laboratory Analytical Instrumentation, Infusion Sets for Parenterals and Drugs, Cosmetic Production, Food and Beverage Processing, Cell and Tissue Culture Transport. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Specific Gravity
- Water Absorption
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- 100% Modulus
- Tear Strength
- Compression Set, Elevated Temperature
- Tensile Set
- Dielectric Strength
- Maximum Service Temperature, Air
- Brittleness Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|