Saint-Gobain Norton® Tygon® Pressure Tubing Formulation B-44-4X I.B.
Subcategory: Thermoplastic
Material Notes: Description: Tygon® B-44-4X I.B. : Tygon® Pressure Tubing's unique flexibility gets it into service quickly and easily. This means less tubing footage, fittings and labor than required for rigid systems. Reinforced with a tough polyester inner-braid imbedded in the wall, it can handle four times the pressure of non-reinforced tubing. Tygon® Pressure Tubing is compatible with virtually all non-solvent chemicals, meeting the needs of many industries in hundreds of applications where flexibility and higher pressure are required. Its clear wall permits positive flow monitoring and inspection. The smooth inner bore of Tygon® Pressure Tubing (smoother than virtually all stainless steel) will not trap bacteria-harboring particles, making it ideal for food and beverage use. It is non-toxic, odorless, taste-free and exhibits outstanding resistance to the alkaline cleaners used in this industry.
Features/Benefits:- Handles four times the pressure of non-reinforced tubing
- Smooth, non-porous bore resists particle entrapment
- Clear wall enables visualization of fluid flow
- Connects easily to Tygopure™ sanitary fittings
- Meets FDA, 3-A and NSF criteria
Typical applications include Cosmetic Production, Food and Dairy Processing, Beverage Dispensing, Pharmaceutical Filling, Water Purification Systems, Printing Equipment, Coolant Lines, Chemical Transfer, Instrumentation and Air Supply Information provided by Saint Gobain Performance Products.
| Available Properties |
- Specific Gravity
- Water Absorption
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- 100% Modulus
- Tear Strength
- Compression Set, Elevated Temperature
- Tensile Set
- Dielectric Strength
- Maximum Service Temperature, Air
- Brittleness Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|