Saint-Gobain Norton® Tygothane® Precision Polyurethane Tubing Formulation C-210-A

 

Subcategory: Polyurethane, TP; Thermoplastic

Material Notes:
Description: Tygothane® C-210-A: Our rigidly controlled manufacturing process makes Tygothane® Precision Polyurethane Tubing the flexible polyurethane tubing that has consistently tight tolerances from lot to lot. Precision tolerances and high elasticity provide the user with an easy, worry-free attachment to fittings. Made of a tough, ester-based polyurethane, Tygothane® Precision Polyurethane Tubing's clarity, high tear strength and excellent abrasion resistance make it ideal for many applications, including fuel and lubricant lines, pneumatic lines, abrasive product transfer and cable jacketing. It also offers exceptional resistance to oils, greases, fuels and many chemicals. Able to withstand rugged daily use, Tygothane® Precision Polyurethane Tubing resists weathering and can be safely used in temperatures ranging from -100°F (-73°C) to 200°F (93°C). It meets FDA criteria for food and beverage use and is also available in ether-based, medical grade and reinforced formulations.

Features/Benefits:

  • Consistently tight dimensional tolerances
  • Excellent abrasion and tear resistance
  • Excellent resistance to oils, greases and fuels
  • High tear resistance
  • Retains flexibility in sub-zero environments
  • Meets FDA criteria
Typical applications include Food and Cosmetic Processing, Abrasive and Viscous Slurry Transfer, Lubrication and Degreaser Dispensing, pellet and Powder Transfer, Pneumatic Sensory Devices, Instrumentation Control Lines, Coolant Recovery Systems
Information provided by Saint Gobain Performance Products.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Hardness, Shore A
  • Tensile Strength, Yield
  • Elongation at Break
  • 100% Modulus
  • 300% Modulus
  • Tear Strength
  • Compression Set, Elevated Temperature
  • Tensile Set
  • Dielectric Strength
  • Maximum Service Temperature, Air
  • Brittleness Temperature
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。