Saint-Gobain Norton® Tygothane® Precision Polyurethane Tubing Formulation C-210-A
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: Description: Tygothane® C-210-A: Our rigidly controlled manufacturing process makes Tygothane® Precision Polyurethane Tubing the flexible polyurethane tubing that has consistently tight tolerances from lot to lot. Precision tolerances and high elasticity provide the user with an easy, worry-free attachment to fittings. Made of a tough, ester-based polyurethane, Tygothane® Precision Polyurethane Tubing's clarity, high tear strength and excellent abrasion resistance make it ideal for many applications, including fuel and lubricant lines, pneumatic lines, abrasive product transfer and cable jacketing. It also offers exceptional resistance to oils, greases, fuels and many chemicals. Able to withstand rugged daily use, Tygothane® Precision Polyurethane Tubing resists weathering and can be safely used in temperatures ranging from -100°F (-73°C) to 200°F (93°C). It meets FDA criteria for food and beverage use and is also available in ether-based, medical grade and reinforced formulations.
Features/Benefits:- Consistently tight dimensional tolerances
- Excellent abrasion and tear resistance
- Excellent resistance to oils, greases and fuels
- High tear resistance
- Retains flexibility in sub-zero environments
- Meets FDA criteria
Typical applications include Food and Cosmetic Processing, Abrasive and Viscous Slurry Transfer, Lubrication and Degreaser Dispensing, pellet and Powder Transfer, Pneumatic Sensory Devices, Instrumentation Control Lines, Coolant Recovery Systems Information provided by Saint Gobain Performance Products.
| Available Properties |
- Specific Gravity
- Water Absorption
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Compression Set, Elevated Temperature
- Tensile Set
- Dielectric Strength
- Maximum Service Temperature, Air
- Brittleness Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|