Saint-Gobain Chemlam® Silver Ultra 3320 High Mechanical Performance Industrial Laminate
Subcategory: Thermoplastic; PTFE
Material Notes: Description: Chemlam® Silver Ultra is the best mechanically performing series of Chemfab® industrial laminates. Chemlam® Silver Ultra composites feature uniform thickness, multi-layer cast PTFE films laminated to fiber glass reinforcements. Chemfab® laminates outperform traditional PTFE-coated products of similar weight and thickness. FEATURES: PTFE cast barrier film surface, crack and pinhole free:Outperforms simple PTFE-coated materials; long-lasting release properties make cleaning easier; low wicking of product into fabric extends useful life. Uniform film thickness over entire surface: Lamination eliminates the possibility of thin spots found in coated materials, which often lead to their premature failure. Bi-colored laminate: Attractive silver top surface is similar in appearance to PTFE cookware; black bottom surface gives clean appearance to composite. High temperature, multi-ply fabrics: Exceptional mechanical properties and dimensional stability at any thickness due to the "plywood" effect; designed for thermal cycling and harsh chemical applications, including cooking and plastic processing. FDA Compliant: Suitable for use in direct food contact applications under the applicable requirements of 21CFR177.1550. All data based on a 0.011 inch test sample. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Specific Gravity
- Tear Strength Test
- Tear Strength
- Color
- Weight (oz/yd^2)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|