Saint-Gobain Chemlam® Ultra 3300 Multi-plied, Flexible, Non-porous Fluoropolymer Laminated Composite
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes: Description: Chemlam® Ultra® is the trademark for the Chemfab® family of multi-plied, flexible, non-porous fluoropolymer laminated composites that combine the feature of multi-layer fluoropolymer cast films with the mechanical properties of fiber glass reinforced fabric. The Ultra® product line offers high performance in severe thermal cycling, chemical applications. FEATURES: PTFE cast barrier film surface, crack and pinhole free:Outperforms simple PTFE-coated materials; long-lasting release properties make cleaning easier; low wicking of product into fabric extends useful life. Uniform film thickness over entire surface: Lamination eliminates the possibility of thin spots found in coated materials, which often lead to their premature failure. Thick gauge films with hardened surfaces: Extended abrasion and wear properties result in longer life with less maintenance. High temperature, multi-ply fabrics: Exceptional mechanical properties and dimensional stability at any thickness due to the "plywood" effect; designed for thermal cycling and harsh chemical applications, including cooking and plastic processing. FDA Compliant: Suitable for use in direct food contact applications under the applicable requirements of 21CFR177.1550. All data based on a 0.0088 inch test sample. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Specific Gravity
- Tear Strength Test
- Tear Strength
- Color
- Weight (oz/yd^2)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|