Saint-Gobain COHRlastic® 9030 Wide Series General Purpose Silicone Solid Rubber
Subcategory: Silicone; Elastomer, TPE; Thermoplastic
Material Notes: Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durometer to the relatively hard 70 durometer on the Shore A scale. It is manufactured in different formulations to provide a choice of physical properties and cost considerations. Series 9030-9070: COHRlastic 9030 - 9070 series is also general purpose (similar to 300 - 700 series), but is produced in 36" wide continuous lengths for the most efficient utilization of material, minimizing waste. Standard thicknesses are 1/32", 1/16" and 1/8". Withstands temperatures from -100°F to 500°F. RED in color.All data based on a 0.0625 inch test sample.(Also comes in thicknesses from 1/32" to 1/8") Information provided by Saint Gobain Performance Products.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Tear Strength
- Compression Set, Elevated Temperature
- Dielectric Strength
- CTE, linear 68°F
- Specific Heat Capacity
- Thermal Conductivity
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|