Saint-Gobain COHRlastic® R10480 Soft Low Compression Set Silicone Sponge Rubber
Subcategory: Silicone; Elastomer, TPE; Thermoplastic
Material Notes: Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R10480 has extremely low compression set and maintains its resiliency even under extended compression. Specification Notes: Meets Specifications: MIL-R-6130 Type II, Grade B&C. All data based on a 0.125 inch test sample.(Other thicknesses available.) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Compressive Strength
- Compression Set
- Dielectric Strength
- CTE, linear 68°F
- Specific Heat Capacity
- Thermal Conductivity
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|