Saint-Gobain COHRlastic® R10460 Medium Flame Retardant Silicone Sponge Rubber
Subcategory: Silicone; Elastomer, TPE; Thermoplastic
Material Notes: Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R10460 is flame retardant. When held in a vertical position and exposed to a 2,000°F flame for 12 seconds, there is no residential flame and less than a 10 second afterglow. Like R10480, it is especially resistant to compression set. Specification Notes: Meets Specifications: AMS 3195, MIL-R-6130 Type II, Grade B&C, MIL-R-46089, Boeing BMS 1-23, Boeing BMS 1-60 Type I, Grade B, Douglas DMS 1597, Douglas DMS 1980, Grade 2, MIL-R-6130 Type II, Grade A. All data based on a 0.0625 inch test sample.(Other thicknesses available.) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Compressive Strength
- Compression Set
- Dielectric Strength
- CTE, linear 68°F
- Specific Heat Capacity
- Thermal Conductivity
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|