Saint-Gobain COHRlastic® R10450 Medium Fiberglass Reinforced Silicone Sponge Rubber
Subcategory: Silicone; Elastomer, TPE; Thermoplastic
Material Notes: Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R10450 silicone sponge with fiberglass reinforcement is a unique construction. It has the compressibility of sponge, plus dimensional stability in the X-Y direction. The absence of stretch contributes to the consistent size and shape of die cut parts and eliminates outward extrusion under pressure. All data based on a 0.0625 inch test sample.(Other thicknesses available.) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Compressive Strength
- Compression Set
- Dielectric Strength
- CTE, linear 68°F
- Specific Heat Capacity
- Thermal Conductivity
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|