Saint-Gobain COHRlastic® Strip-N-Stick® 100S Silicone Sponge/High Temp Silicone Adhesive Pressure Sensitive Tape
Subcategory: Silicone; Adhesive; Tape; Thermoplastic
Material Notes: Description: Strip-N-Stick® tape provides all the benefits of silicone rubber in an easy-to-apply, pressure-sensitive adhesive tape form. Compressible and flexible, it can conform to irregular surfaces, wrap over cylinders or be formed to produce right angles. Applications include gasketing, vibration damping, and thermal insulation. The tape reduces the need for expensive die-cut-parts--you don't pay for the center. It also eliminates the high cost of bonding and will be slit to order for 1/2" and up. 100S is a silicone sponge with high temperature silicone adhesive. Adhesive temperature range for Silicone PSA is -100°F to +500°F and for Acrylic PSA, -20°F to 300°F. Base material is R10470M. Silicone rubber material type is sponge. Adhesive type is silicone. All data based on a 0.0625 inch test sample.(Other thicknesses available.) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Tensile Strength, Yield
- Elongation at Break
- Compressive Strength
- Compression Set, Elevated Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|