Saint-Gobain CHR® 2302-5R UHMW Film Backing Acrylic Adhesive Pressure Sensitive Tape

 

Subcategory: Adhesive; Acrylic; Tape; Thermoplastic

Material Notes:
Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications include bearings, chute and guide rail coverings. This tape uses an acrylic adhesive system. Acrylic adhesves perform in continuous operating temperatures from -40°F to +375°F (-40°C to +188°C). Benefits include exceptional solvent resistance, excellent adhesion to metal, superior weathering and aging characteristics. Acrylics have an excellent shelf life, and when exposed to elevated temperatures, their ability to wet-out improves thus increasing both adhesion and tack properties. All data based on a 0.0065 inch test sample.(Thickness given is for both backing and adhesive. Backing thickness is .005 inches.)
Information provided by Saint Gobain Performance Products.

Available Properties
  • Elongation at Break
  • Tear Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。