Saint-Gobain CHR® 2819-5(R) Acrylic Adhesive Zone Tape
Subcategory: Adhesive; Acrylic; Tape; Thermoplastic
Material Notes: Specification Notes: 21CFR177.1550 compliant. All data based on a 0.0047 inch test sample. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Elongation at Break
- Tear Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|