Saint-Gobain CHR® C680 Paper Backing Silicone Adhesive Pressure Sensitive Tape
Subcategory: Silicone; Adhesive; Tape; Thermoplastic
Material Notes: Description: Paper tapes are designed to provide high temperature and excellent solvent resistance for wave soldering, printed circuit board masking, and hot air leveling applications. Service temperatures range from -100°F to 500°F (-73°C tp +260°C). This tape uses a silicone adhesive system. Perfect for extreme temperature applications, silicone adhesives perform in continuous operating temperatures from -100°F to 500° (-73°C to 260°C). Silicone-based adhesive systems exhibit good chemical resistance, retain electrical properties, and remove cleanly with little or no residue. All data based on a 0.006 inch test sample.(Thickness given is for both backing and adhesive. Backing thickness is .004 inches.) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Elongation at Break
- Tear Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|