Saint-Gobain Norton® Norseal® V770 Low-Density Pressure Sensitive Adhesive Sealant Foam
Subcategory: Vinyl; Adhesive; Thermoplastic
Material Notes: Description: Low Density Foam Suitable for Sealing of Thin Gauge Metals and Plastics. Closed cell polyvinyl chloride foam sealant with pressure sensitive adhesive on one side. The tight bonding adhesive keeps sealant in place during each stage of product assembly. The adhesive is on the non-linear side, making installation easier and quicker.
Features/Benefits:- 30% compression provides an excellent seal against light, dust and water in mechanically fastened assemblies
- Excellent resistance to weather, fungi, and oxidation provides a long sealing life
- Will not crack in cold temperatures
- Superb closed cell structure of foam provides a positive seal
- Low force to compress means faster and easier formation of a positive seal
- Flexibility facilitates use in radius corners
- Low density sealant allows easy assembly of large wall systems
Typical Applications: Curtainwall, precast concrete walls, refridgeration, telecommunications, pheumatic system seals, retail weatherstrip, bus and off-road vehicles, air conditioning, environmentally controlled rooms. All data based on a 0.25 inch test sample.(Available in thicknesses from 1/8" to 1/2".) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore OO
- Tensile Strength, Yield
- Elongation at Break
- Compressive Strength
- Compressive Modulus
- Compression Set
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|