Saint-Gobain Norton® Norseal® V780 Medium-Density Pressure Sensitive Adhesive Sealant Foam
Subcategory: Adhesive; Thermoplastic
Material Notes: Description: Improved Performance: Norseal® V780 medium density foam sealant combines a closed cell foam substrate with a one-sided pressure-sensitive adhesive. Norseal has been specially formulated to provide superior performance with a reduced density foam, and is ideal for applications such as small appliance seals, corrugated wall seals, machinery enclosures, buses and off-road vehicles, HVAC seals, and window and door seals.
Closed Cell Foam: Meets FMVSS 302 Flammability Standard; Superb closed cell structure of foam uses less material to achieve a positive seal; Consistent seal with a minimum of 30% compression; Available in black.
Pressure-Sensitive Adhesive: High performance adhesive coating eliminates messy adhesive application; Liner is on the non-adhesive side. The roll stays together during handling with no stretching when applied.
Medium Density: Specially formulated to provide high performance with a reduced density foam; Excellent weathering, oxidation and fungi resistance provides long life; Formulated to prevent water infiltration on irregular surfaces.
Features/Benefits: Multipurpose medium density closed cell foam uses less material to achieve a positive seal; Meets FMVSS 302 Flammability Standard; Prevents water infiltration on irregular surfaces; Resistant to weather, Fungi and Oxidation; Broad service temperature range; Dimensionally stable.
Typical applications include: Corrugated wall seals, lighting equipment, small appliances, door and window seals, machinery enclosures, buses and off-road vehicles, concrete forms, HVAC seals. All data based on a 0.25 inch test sample.(Available in thicknesses from 1/16" to 3/8".) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore OO
- Tensile Strength, Yield
- Elongation at Break
- Compressive Strength
- Compressive Modulus
- Compression Set
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|