Saint-Gobain Lo-Skid® LS7000/LS7100 Series High Density Bumper and Footpad Urethane Foam
Subcategory: Adhesive; Polyurethane, TP; Acrylic; Thermoplastic
Material Notes: Description: Lo-Skid™ LS7000 and LS7100 (acrylic adhesive on one side) urethane foam products are widely recommended for bumpers and footpads for applications and electronic products because it provides a high coefficient of surface friction combined with a smooth non-marring surface. Lo-Skid is flexible and can be die-cut to the required size and shape. Features/Benefits: High coefficient of friction; Abrasion resistance; Flexible and conformable; High durometer - will withstand heavy loads; Smooth, non-marring surface; Thicknesses from 16 mils to 125 mils. Typical Applications: Foot pads and bumpers for business machines, housewares, industrial equipment, electronics. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Hardness, Shore O
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Compressive Modulus
- Coefficient of Friction
- Tear Strength
- Compression Set
- Compression Set, Elevated Temperature
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|