Saint-Gobain Norton® Norseal® V760 High Density Vibration Dampening Foam Sealant
Subcategory: Vinyl; Thermoplastic
Material Notes: Description: Seals and Dampens Vibration: Norseal® V760 is a closed-cell PVC foam sealant with a pressure-sensitive adhesive on one side. Its high-density structure and multitude of tiny cells act like shock absorbers to seal and dampen vibration. Firm, High Density Foam for Positive Seals: This shock-absorbing feature makes Norseal V760 ideal for die-cut applications and metal-to-metal sealing. Versatile and easy to use, Norseal V760 is designed to produce a positive seal in mechanically fastened assemblies with as little as 30 percent compression. Conformable and Dimensionally Stable: Norseal V760 provides excellent conformability to curved and irregular shapes. It is resistant to weather, fungi and oxidation, ensuring a long sealing life. In addition, Norseal V760 is dimensionally stable. It will not drip, ooze or run under compression, and remains flexible at low temperatures. Pressure Sensitive Adhesive: The aggressive pressure-sensitive adhesive on one side of Norseal V760 facilitates high-speed application. The easy-peel paper liner eliminates stretching during installation, and removes easily after application. Norseal V760 series is available in gray. For specific low energy plastics, a specially formulated adhesive, "LE" is available.
FEATURES/BENEFITS:- Dimensionally stable under compression
- Good abrasion resistance
- Design facilitates high-speed application
- Liner removes easily after application
- Resistant to wether, fungi and oxidation
- Low water absorption for long sealing life
- Provides insulating properties
Applications: Truck trailer joint seals, door frame assemblies, concrete forms, export container seals, die-cut gaskets, roof sealing for parapets, duct seals, appliance seals, truck cab overlap seals. All data based on a 0.125 inch test sample.(Available in multiple thicknesses.) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore OO
- Tensile Strength, Yield
- Elongation at Break
- Compressive Strength
- Compressive Modulus
- Compression Set
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|