Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture
Subcategory: Thermoplastic
Material Notes: Features/Benefits:- Outlasts silicone tubing in peristaltic pumps by up to 30 times
- Low particulate spallation
- Can be autoclaved repeatedly
- Temperature resistant from -60°F to 275°F
- Withstands repeated CIP and SIP cleaning and sterilization
- Fully tested to ISO 10993 standards to facilitate validation process
- Meets USP Class VI FDA and NSF criteria
Typical Applications include: Diagnostic test product manufacturing, cell harvest and media process systems, vaccine manufacturing, bioreactor process lines, production filtration and fermentation, sterile filling, shear sensitive fluid transfer. UL94-HB Flame Resistance Classification Passed. All data based on a 0.0625 inch test sample.(Available in multiple thicknesses.) Information provided by Saint Gobain Performance Products.
| Available Properties |
- Specific Gravity
- Water Absorption
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Tear Strength
- Compression Set
- Tensile Set
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|