Saint-Gobain Chemlam® Copper SGC6-10 Adhesive Tape
Subcategory: Adhesive; Tape; Thermoplastic; PTFE
Material Notes: Description: Chemlam® Copper SGC6 is fiberglass fabric impregnated with PTFE (polytetrafluoroethylene) dispersion, laminated to PTFE film and coated with high-temperature, pressure-sensitive silicone adhesive.
Backing material: PTFE coated fiberglass fabric Adhesive Type: Clean Release Silicone. All data based on a 0.0114 inch test sample. Information provided by Saint Gobain Performance Products.
| Available Properties |
- Elongation at Break
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|