STRUKTOL® TR 255 Processing Additive, Dispersant
Subcategory: Additive/Filler for Polymer
Close Analogs: FDA Status: 173.340; 175.105; 175.300; 175.320; 176.170; 176.200; 176.210; 177.1200; 177.2260; 177.2410; 177.2600; 178.2010; 178.3860; 181.29; 184.1229
Material Notes: A complex oleochemical mixture containing mono and di amides and metal soap.STRUKTOL® TR 255 is a unique blend of surfactant and lubricant components designed for applications where EBS (ethyl bis-stearamide) is commonly used. These include ABS compounds, rigid PVC extrusions, color concentrates and other high-filled applications, such as calcium carbonate-filled polypropylene. STRUKTOL® TR 255 has enhanced functionality over EBS with similar gloss properties. It is manufactured from raw materials that enable the finished product to meet requirements for FDA sanction.
| Available Properties |
- Specific Gravity
- Additive Loading
- Dropping Point
- Shelf Life
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|