STRUKTOL® CALCIUM STEARATE
Subcategory: Additive/Filler for Polymer
Close Analogs: FDA Status: 173.340; 175.105; 175.300; 175.320; 176.170; 176.200; 176.210; 177.1200; 177.2260; 177.2410; 177.2600; 178.2010; 181.29; 184.1229
Material Notes: High purity, non-wettable, calcium stearate powder manufactured with high quality stearic acid.STRUKTOL® Calcium Stearate is used by the rubber and plastic industries as an effective elastomer processing aid and release agent. The low chloride content of STRUKTOL® Calcium Stearate allows for complete product dispersion in elastomers. STRUKTOL® Calcium Stearate reduces extruder pressure build-up of rigid PVC compounds when used as a processing aid during the manufacture of pipe, siding and injection molded fittings. The low chloride content of STRUKTOL® Calcium Stearate meets the quality and processing demands of polyolefin, polystyrene and polyester manufacture. STRUKTOL® Calcium Stearate can also be used as a processing aid in wire drawing operations, and as an anti-caking additive in dry blending operations. Some of the benefits of using STRUKTOL® Calcium Stearate are: - LOW DUST Controlled particle size during manufacture significantly reduces fines and virtually eliminates work area dust problems. - EASY HANDLING Eliminates bridging or caking while facilitating use in any type of packaging, bulk handling or conveying system. - LOW IMPURITY Reduces extruder pressure build-up and minimizes fiber breakage during extrusion and spinning. - COLOR STABILITY High-purity and a unique manufacturing process give this product extreme heat resistance to prevent discoloration and haze formation.
| Available Properties |
- Specific Gravity
- Additive Loading
- Particle Mesh Size
- Ash
- Melting Point
- Moisture Content
- Appearance
- Free Fatty Acid (%, max)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|